Bitte benutzen Sie diese Kennung, um auf die Ressource zu verweisen: http://dx.doi.org/10.25673/118316
Titel: Effect of surface treatment strategies on bond strength of additively and subtractively manufactured hybrid materials for permanent crowns
Autor(en): Mao, Zhen
Schmidt, Franziska
Beuer, FlorianIn der Gemeinsamen Normdatei der DNB nachschlagen
Yassine, Jamila
Hey, JeremiasIn der Gemeinsamen Normdatei der DNB nachschlagen
Prause, Elisabeth
Erscheinungsdatum: 2024
Art: Artikel
Sprache: Englisch
Zusammenfassung: Objectives: The purpose of this study is to evaluate the bond strength of different computer-aided design / computer-aided manufacturing (CAD/CAM) hybrid ceramic materials following different pretreatments. Methods: A total of 306 CAD/CAM hybrid material specimens were manufactured, n = 102 for each material (VarseoSmile Crownplus [VSCP] by 3D-printing; Vita Enamic [VE] and Grandio Blocs [GB] by milling). Each material was randomly divided into six groups regarding different pretreatment strategies: control, silane, sandblasting (50 μm aluminum oxide particles), sandblasting + silane, etching (9% hydrofluorics acid), etching + silane. Subsequently, surface roughness (Ra) values, surface free energy (SFE) were measured. Each specimen was bonded with a dual-cured adhesive composite. Half of the specimens were subjected to thermocycling (5000 cycles, 5–55 °C). The shear bond strength (SBS) test was performed. Data were analyzed by using a two-way analysis of variance, independent t-test, and Mann-Whitney-U-test (α = 0.05). Results: Material type (p = 0.001), pretreatment strategy (p < 0.001), and the interaction (p < 0.001) all had significant effects on Ra value. However, only etching on VSCP and VE surface increased SFE value significantly. Regarding SBS value, no significant difference was found among the three materials (p = 0.937), while the pretreatment strategy significantly influenced SBS (p < 0.05). Etching on VSCP specimens showed the lowest mean value among all groups, while sandblasting and silane result in higher SBS for all test materials. Conclusions: The bond strength of CAD/CAM hybrid ceramic materials for milling and 3D-printing was comparable. Sandblasting and silane coupling were suitable for both millable and printable materials, while hydrofluoric etching should not be recommended for CAD/CAM hybrid ceramic materials. Clinical relevance: Since comparable evidence between 3D-printable and millable CAD/CAM dental hybrid materials is scarce, the present study gives clear guidance for pretreatment planning on different materials.
URI: https://opendata.uni-halle.de//handle/1981185920/120275
http://dx.doi.org/10.25673/118316
Open-Access: Open-Access-Publikation
Nutzungslizenz: (CC BY 4.0) Creative Commons Namensnennung 4.0 International(CC BY 4.0) Creative Commons Namensnennung 4.0 International
Journal Titel: Clinical oral investigations
Verlag: Springer
Verlagsort: Berlin
Band: 28
Heft: 7
Originalveröffentlichung: 10.1007/s00784-024-05767-3
Seitenanfang: 1
Seitenende: 12
Enthalten in den Sammlungen:Open Access Publikationen der MLU

Dateien zu dieser Ressource:
Datei Beschreibung GrößeFormat 
s00784-024-05767-3.pdf2.83 MBAdobe PDFMiniaturbild
Öffnen/Anzeigen