Titel: | Mechanical properties of 3D-printed and milled composite resins for definitive restorations : an in vitro comparison of initial strength and fatigue behavior |
Autor(en): | Prause, Elisabeth Malgaj, Tine Kocjan, Andraž Beuer, Florian Hey, Jeremias Jevnikar, Peter Schmidt, Franziska |
Erscheinungsdatum: | 2024 |
Art: | Artikel |
Sprache: | Englisch |
Zusammenfassung: | Objective: To evaluate the flexural strength and fatigue behavior of a novel 3D-printed composite resin for definitive restorations. Materials and Methods: Fifty disc-shaped specimens were manufactured from each of a nanohybrid composite resin (NHC), polymer-infiltrated ceramic network (PICN), and 3D-printed composite resin (3D) with CAD-CAM technology. Biaxial flexural strength (σin) (n = 30 per group) and biaxial flexural fatigue strength (σff) (n = 20 per group) were measured using piston-on-three-balls method, employing a staircase approach of 105 cycles. Weibull statistics, relative-strength degradation calculations, and fractography were performed. The results were analyzed with 1-way ANOVA and Games-Howell post hoc test (α = 0.05). Results: Significant differences in σin and σff among the groups (p < 0.001) were detected. The NHC group provided the highest mean ± standard deviation σin and σff (237.3 ± 31.6 MPa and 141.3 ± 3.8 MPa), followed by the PICN (140.3 ± 12.9 MPa and 73.5 ± 9.9 MPa) and the 3D (83.6 ± 18.5 MPa and 37.4 ± 23.8 MPa) groups. The 3D group exhibited significantly lower Weibull modulus (m = 4.7) and up to 15% higher relative strength degradation with areas of nonhomogeneous microstructure as possible fracture origins. Conclusions: The 3D-printed composite resin exhibited the lowest mechanical properties, where areas of nonhomogeneous microstructure developed during the mixing procedure served as potential fracture origins. Clinical Significance: The clinical indications of the investigated novel 3D-printed composite resin should be limited to long-term provisional restorations. A cautious procedure for mixing the components is crucial before the 3D-printing process, since nonhomogeneous areas developed during the mixing could act as fracture origins. |
URI: | https://opendata.uni-halle.de//handle/1981185920/119219 http://dx.doi.org/10.25673/117260 |
Open-Access: | Open-Access-Publikation |
Nutzungslizenz: | (CC BY-NC-ND 4.0) Creative Commons Namensnennung - Nicht kommerziell - Keine Bearbeitungen 4.0 International |
Journal Titel: | Journal of esthetic and restorative dentistry |
Verlag: | Wiley-Blackwell |
Verlagsort: | Oxford [u.a.] |
Band: | 36 |
Heft: | 2 |
Originalveröffentlichung: | 10.1111/jerd.13132 |
Seitenanfang: | 391 |
Seitenende: | 401 |
Enthalten in den Sammlungen: | Open Access Publikationen der MLU |
Dateien zu dieser Ressource:
Datei | Beschreibung | Größe | Format | |
---|---|---|---|---|
jerd-13132.pdf | 2.85 MB | Adobe PDF | Öffnen/Anzeigen |